Effect of Ekabor 2 powder on the mechanical properties of pure iron powder metal compacts
dc.contributor.author | Altintas, A | |
dc.contributor.author | Sarigün, Y | |
dc.contributor.author | Çavdar, U | |
dc.date.accessioned | 2025-04-10T10:29:28Z | |
dc.date.available | 2025-04-10T10:29:28Z | |
dc.description.abstract | Ekabor 2 powder of different weights, used by V type powder mixture was mixed with pure iron powder. Specimens were created by dry pressing into die followed by cold isostatic press at a pressure of 100 bar for purpose of resizing. The conventional sintering process at 900 degrees C and 950 degrees C was carried out for 4 h using conventional furnaces. Specimens were gradually cooled by air. The sintered pellets were examined in terms of density, wear abrasion, surface roughness and hardness at 900 degrees C and 950 degrees C. Microstructure of pellets was observed with optic microscope. The results show that the hardness gradually increased with additions of 0 wt. % to 10 wt. % of Ekabor 2 however, after 10 wt. %, this hardness tended to decrease. | |
dc.identifier.e-issn | 1988-4222 | |
dc.identifier.issn | 0034-8570 | |
dc.identifier.uri | http://hdl.handle.net/20.500.14701/36196 | |
dc.language.iso | English | |
dc.title | Effect of Ekabor 2 powder on the mechanical properties of pure iron powder metal compacts | |
dc.type | Article |