Wear behavior-hardness-microstructure relation of Fe-Cr-C and Fe-Cr-C-B based hardfacing alloys

dc.contributor.authorYüksel N.
dc.contributor.authorŞahin S.
dc.date.accessioned2024-07-22T08:17:27Z
dc.date.available2024-07-22T08:17:27Z
dc.date.issued2014
dc.description.abstractThe aim of this study is the investigation of the effect of ferroboron and the amount of powder mixture (ferroboron. +. ferrochromium) on wear resistance of Iron (Fe)-Chromium (Cr)-Carbon (C) based hardfacing alloys. Powder mixture, consisting of ferrochromium (FeCr) and ferroboron (FeB), was added to massive wire during welding process. Hardfaced layers were obtained by three different powder mixtures and two different powder/massive wire proportions. Hardfacing was applied to AISI 1020 steel substrate by open arc welding. Hardness test, Scanning Electron Microscope (SEM) and X-Ray Diffraction (XRD) analysis, dry sand/rubber wheel abrasion test were executed. Test results showed that increasing ferroboron content and increasing powder mixture amount enhanced the wear resistance. © 2014 Elsevier Ltd.
dc.identifier.DOI-ID10.1016/j.matdes.2014.02.032
dc.identifier.issn02613069
dc.identifier.urihttp://akademikarsiv.cbu.edu.tr:4000/handle/123456789/17062
dc.language.isoEnglish
dc.publisherElsevier Ltd
dc.subjectBoron
dc.subjectHard facing
dc.subjectHardness
dc.subjectMixtures
dc.subjectScanning electron microscopy
dc.subjectWear resistance
dc.subjectWelding
dc.subjectWire
dc.subjectFerroboron
dc.subjectFerrochromium
dc.subjectHardfacing alloys
dc.subjectOpen arc welding
dc.subjectPowder mixtures
dc.subjectSteel substrate
dc.subjectWear test
dc.subjectWelding process
dc.subjectIron alloys
dc.titleWear behavior-hardness-microstructure relation of Fe-Cr-C and Fe-Cr-C-B based hardfacing alloys
dc.typeArticle

Files