Effect of Ekabor 2 powder on the mechanical properties of pure iron powder metal compacts

dc.contributor.authorAltintaş A.
dc.contributor.authorSarigün Y.
dc.contributor.authorÇavdar U.
dc.date.accessioned2025-04-10T11:09:11Z
dc.date.available2025-04-10T11:09:11Z
dc.date.issued2016
dc.description.abstractEkabor 2 powder of different weights, used by V type powder mixture was mixed with pure iron powder. Specimens were created by dry pressing into die followed by cold isostatic press at a pressure of 100 bar for purpose of resizing. The conventional sintering process at 900 °C and 950 °C was carried out for 4 h using conventional furnaces. Specimens were gradually cooled by air. The sintered pellets were examined in terms of density, wear abrasion, surface roughness and hardness at 900 °C and 950 °C. Microstructure of pellets was observed with optic microscope. The results show that the hardness gradually increased with additions of 0 wt. % to 10 wt. % of Ekabor 2 however, after 10 wt. %, this hardness tended to decrease. Copyright: © 2016 CSIC.
dc.identifier.DOI-ID10.3989/revmetalm.073
dc.identifier.urihttp://hdl.handle.net/20.500.14701/48560
dc.publisherCentro Nacional de Investigaciones Metalurgicas
dc.titleEffect of Ekabor 2 powder on the mechanical properties of pure iron powder metal compacts